Share your shave of the day!

  • gcgallant@sub.wetshaving.social
    link
    fedilink
    arrow-up
    2
    ·
    2 months ago

    Maybe sputtering the edge …

    Yeah, I thought of that too. Normally, that wears away after the first few days, though. (Among the many useful takeaways I’ve had from previous AAs 🙂)

      • gcgallant@sub.wetshaving.social
        link
        fedilink
        arrow-up
        2
        ·
        1 month ago

        Yes. It’s generally gone within the first few days. I think, now, that the added comfort of the sputtered material comes from reducing the harshness of a freshly machined edge.

        • djundjila@sub.wetshaving.socialM
          link
          fedilink
          arrow-up
          2
          ·
          1 month ago

          I’m a bit confused here. My understanding is that the polymer coating is here to increase glide and reduce the harshness. The sputtered tungsten, titanium and whatnot is sputtered onto the edge, under the coating to add wear resistance, but it makes the surface rougher, which I thinkshould translate into a harsher feel.

          • gcgallant@sub.wetshaving.social
            link
            fedilink
            arrow-up
            2
            ·
            1 month ago

            I obviously don’t know, but from videos I’ve seen of making DE blades, the tradeoff between cost and precision favors cost. My assumption on the sputtering is that it normalizes the edge and that the coating reduces harshness when the blade is at its sharpest.

            My scope is calibrated so the 50 micron scale at the bottom left is reasonably accurate. It’s amazing how much better the resolving power of a SEM is at similar magnification.

            After AA I’ll do a sequence with a DE blade. I’ve only done a GEM and Kismet so far.